Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 890000 cP

@Temperature 160 °C
890000 cP

@Temperature 320 °F
Melt viscosity @ 2.16 kg; ISO 1133
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft..