Physical Properties Metric English Comments
Viscosity 85000 - 95000 cP

@Temperature 25.0 °C
85000 - 95000 cP

@Temperature 77.0 °F
Uncured
Permabond TA435 Toughened Acrylic Adhesive & Initiator
PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli..
Viscosity 85000 cP
85000 cP
mix viscosity
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive  (discontinued **)
Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C).
Viscosity 85000 cP

@Temperature 204 °C
85000 cP

@Temperature 399 °F
Melt; ASTM D-1084-88
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S..
Viscosity 85000 cP
85000 cP
mixing, dynamic
Dow Corning SILASTIC® J RTV SILICONE RUBBER BASE & CURING AGENT
High durometer silicone mold making rubber recommended for use with rigid and foam polyurethane and can be used with polyesters and epoxies.Information provided by Dow Corning
Viscosity 85000 cP

@Shear Rate 5000 1/s,
Temperature 295 °C
85000 cP

@Shear Rate 5000 1/s,
Temperature 563 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..