Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive  (discontinued **)

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C).
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
Viscosity 85000 cP
85000 cP
mix viscosity
Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.30 MPa
1200 psi
Per ASTM D1002-94; shear strength of single lap-joint metal coupons in tension loading.
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.80 W/m-K
12.5 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1e+05
1e+05
Dielectric Strength 2.00 kV/mm
50.8 kV/in
Processing Properties Metric English Comments
Pot Life 45 - 60 min
45 - 60 min