Physical Properties Metric English Comments
Viscosity 85 cP
85 cP
Formic Acid Viscosity; ISO Test
BASF Capron® B85ZP Nylon 6 (DAM) (America)  (discontinued **)
Not Impact modified.Information provided by BASF.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Viscosity 85 cP
85 cP
LG Chemical LGflex GL100 Plasticizer
Features: Excellent Heat Loss and Non-endocrine disrupter Application: PVC Power Cable, SheetsInformation provided by LG Chemical
Viscosity 85 cP
85 cP
KKPC KOSYN KSL 202 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro..
Viscosity 85 - 100 cP
85 - 100 cP
Huntsman Araldite ECN 1299 Epoxy Cresol Novolac
Weight per Epoxide (EEW, g/eq) 217 to 244. Max color is
Viscosity 85 cP
85 cP
Elmer's Products Aron Alpha® 202F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Viscosity 85 cP
85 cP
Elmer's Products Aron Alpha® 802 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Medium gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrate..
Viscosity 85 - 105 cP
85 - 105 cP
ASTM D445
ExxonMobil Jayflex™ DINP Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaCAS Number: 68515-48-0EC Number: 271-090-9Information provided by ExxonMobil
Viscosity 85 cP
85 cP
Solvay RHODAFAC® ASI-80 Octyl phosphonic acid
Identification: ALKYL PHOSPHONATE DERIVATIVECAS: 4724 – 48 – 5EINECS: 225 – 218 – 5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Corrosion inhibitor for ferrou..