LG Chemical LGflex GL100 Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer LG Chemical
Trade Name LGflex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LGflex GL100 Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent Heat Loss and Non-endocrine disrupter Application: PVC Power Cable, SheetsInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.973 - 0.979 g/cc
0.973 - 0.979 g/cc
Volatiles 2.2 %

@Time 3600 sec
2.2 %

@Time 1.00 hour
Loss
4.7 %

@Time 7200 sec
4.7 %

@Time 2.00 hour
Loss
Viscosity 85 cP
85 cP
Molecular Weight 404 g/mol
404 g/mol
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
Elongation at Break 410 %
410 %
50% Modulus 0.00637 GPa
0.924 ksi
100% Modulus 0.0103 GPa
1.49 ksi
Thermal Properties Metric English Comments
Melting Point -45.0 °C
-49.0 °F
Freezing Point
Boiling Point 400 - 416 °C
752 - 781 °F
Flash Point 252 °C
486 °F
Optical Properties Metric English Comments
Refractive Index 1.483 - 1.489
1.483 - 1.489
Electrical Properties Metric English Comments
Volume Resistivity >= 2.00e+11 ohm-cm
>= 2.00e+11 ohm-cm
Chemical Properties Metric English Comments
Acid Value <= 0.030
<= 0.030
KOH mg/g
<= 0.070
<= 0.070
After Heating, KOH mg/g
Descriptive Properties Value Comments
Color <20 APHA
Flexible Temperature -9 kg/cm2
G=3.17x10<sup>3<sup>
Heat Loss <0.07%