Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.0 - 7.5 cP | 3.0 - 7.5 cP | |
Daikin NEOFLON ND-4GY FEP Dispersion, Gray NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |