Physical Properties Metric English Comments
Viscosity 66000 cP

@Temperature 25.0 °C
66000 cP

@Temperature 77.0 °F
Mixed (rv #7, 10 rpm)
Tra-Con Tra-Bond 216E02 Encapsulant for "Fill" Applications
TRA-BOND 216E02 is a two-part epoxy adhesive developed specifically for underfill and encapsulating applications where the combination of excellent mechanical, thermal and electrical properties are ..
Viscosity 66000 cP
66000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Viscosity 66000 cP
66000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Viscosity 66000 cP
66000 cP
Melt Viscosity, 280°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics NORYL PX2060 PPE+PS