Polymer Property : Viscosity = 62000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 62000 cP
62000 cP
Mixed (cp #52, 5 rpm)
Tra-Con Tra-Duct 921U02 Long Pot Life Silver-Filled Epoxy
TRA-DUCT 921U02 long room temperature pot life, silver-filled epoxy. Information provided by Tra-Con Inc.