Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 70000 - 6.00e+6 cP | 70000 - 6.00e+6 cP | |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Viscosity | 100000 - 6.00e+6 cP | 100000 - 6.00e+6 cP | |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Viscosity | 100000 - 6.00e+6 cP | 100000 - 6.00e+6 cP | |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |