Viscosity 4400 - 5600 cP
4400 - 5600 cP
Huntsman Tactix 123 Epoxy
Weight per Epoxide (EEW, g/eq) 172 to 176.Comments/Applications: Very low viscosity bisphenol-A based epoxy resin for applications such as filament winding.Data provided by Ciba Specialty Chemicals...