Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4400 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
4400 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2090512D1 70:30 Silver Palladium Ink C2090512D1 is an ink based on a 70:30 ratio of Silver:Palladium. It is designed as an internal electrode ink for use with PVB tape. Screen Printing Equipment: semi-automatic, manualScreen Types: sta.. |
|||
Viscosity | 4400 - 5600 cP | 4400 - 5600 cP | |
Huntsman Tactix 123 Epoxy Weight per Epoxide (EEW, g/eq) 172 to 176.Comments/Applications: Very low viscosity bisphenol-A based epoxy resin for applications such as filament winding.Data provided by Ciba Specialty Chemicals... |
|||
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G201 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G210 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 4400 - 5200 cP @Temperature 35.0 °C |
4400 - 5200 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G202 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |