Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 520000 cP | 520000 cP | |
Dow Corning SILASTIC® 9280/75E KIT PARTS A&B 60 Durometer, 2-part, 1 to 1 mix, translucent, injection moulding grade, Liquid Silicone Rubber.Information provided by Dow Corning |