Polymer Property : Viscosity = 51500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 51500 cP
51500 cP
10.0 rpm; TM R050-12
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..