Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.30 - 51.0 cP | 3.30 - 51.0 cP | Average value: 11.2 cP Grade Count:14 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |