Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.60 - 50.0 cP | 2.60 - 50.0 cP | Average value: 18.4 cP Grade Count:3 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Viscosity | 2.60 - 50.0 cP | 2.60 - 50.0 cP | Average value: 9.37 cP Grade Count:7 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 2.60 - 50.0 cP | 2.60 - 50.0 cP | Average value: 8.83 cP Grade Count:17 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Viscosity | 2.60 - 50.0 cP | 2.60 - 50.0 cP | Average value: 18.4 cP Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |