Polymer Property : Viscosity = 50.0 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 18.4 cP Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 9.37 cP Grade Count:7
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 8.83 cP Grade Count:17
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 18.4 cP Grade Count:3
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..