Physical Properties Metric English Comments
Viscosity 48000 cP

@Shear Rate 100 1/s,
Temperature 25.0 °C
48000 cP

@Shear Rate 100 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Gwent Electronic Materials C2010829D2 Silver Ink
Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has be..
Viscosity 48000 cP

@Temperature 25.0 °C
48000 cP

@Temperature 77.0 °F
Mixed (10 rpm)
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound
TRA-BOND 2159 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards..