Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 475000 cP @Temperature 400 °C |
475000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Viscosity | 475000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
475000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 475000 cP @Temperature 400 °C |
475000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |