Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 460 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 460 - 1200 cP
460 - 1200 cP
Huntsman HY 3150 Aromatic Amine
Approx. H+ equivalent weight 58. Mix Ratio with GY 6010 is 23.Comments/Applications: High solids coatings, floorings and tank linings. Good acetic acid resistance and other aggressive environment..
Viscosity 460 - 680 cP
460 - 680 cP
NOV QC 020
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Copyright © lookpolymers.com All Rights Reserved