Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2200 - 4300 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2200 - 4300 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2030408P3 Carbon Graphite Ink This product is designed to be used for screen printing working electrodes. This is a carbon/graphite ink which has been optimized to give superior electrochemical performance and contains Cobalt Ph.. |
|||
Viscosity | 3300 - 4300 cP @Temperature 25.0 °C |
3300 - 4300 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-08 MDI Isocyanate Description of product: 4,4`-diphenyl-methane-diisocyanate and polyether-diol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for producing e.. |