Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 430 cP | 430 cP | dynamic |
Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL Two-parts, clear, RT or heat cure.Information provided by Dow Corning |
|||
Viscosity | 430 cP @Temperature 25.0 °C |
430 cP @Temperature 77.0 °F |
|
Dow SPECTRIM™ MM 310-B Polyol SPECTRIM™ MM 310-B multi-component formulated polyol is a component of SPECTRIM™ MM 310 reaction moldable polymer.Information provided by Dow |
|||
Viscosity | 430 cP | 430 cP | dynamic |
Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning |