Physical Properties Metric English Comments
Viscosity 390000 cP

@Shear Rate 190 1/s,
Temperature 230 °C
390000 cP

@Shear Rate 190 1/s,
Temperature 446 °F
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer
Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Viscosity 390000 cP
390000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
Viscosity 390000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
390000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..