Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 90000 - 380000 cP | 90000 - 380000 cP | Average value: 183000 cP Grade Count:4 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |