Polymer Property : Viscosity = 370 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 370 cP

@Temperature 40.0 °C
370 cP

@Temperature 104 °F
25% in dimethylacetamide; Internal Method
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s..
Viscosity 370 cP
370 cP
Solution Viscosity; ASTM D455
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth..
Viscosity 370 cP
370 cP
Dow Corning SYL-OFF® 7610 COATING
Syl-Off® 7610 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. General purpose coating with exceptiona..
Viscosity 370 cP
370 cP
Dynamic
Dow Corning SYL-OFF® PMCP7610 Coating
Syl-Off® 7610 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. General purpose coating with exceptiona..
Viscosity 370 cP
370 cP
Aremco Ceramabind™ 642 High Temperature Inorganic Binder
A basic solution which is highly compatible with most ceramic and metal powders. Good wettability and tack, and excellent acid resistance after curing. Extremely moisture resistant after a high temp..