Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 32000 - 36000 cP @Temperature 23.0 °C |
32000 - 36000 cP @Temperature 73.4 °F |
|
Master Bond UV21 One Component Highly Flexible UV Curable Urethane Elastomer Master Bond Polymer System UV21 is an easy to use one component UV curable urethane elastomer compound. It has been used for bonding, sealing, casting and formed in place high
performance seals and .. |