Master Bond UV21 One Component Highly Flexible UV Curable Urethane Elastomer

Category Polymer , Adhesive , Thermoset
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV21 One Component Highly Flexible UV Curable Urethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System UV21 is an easy to use one component UV curable urethane elastomer compound. It has been used for bonding, sealing, casting and formed in place high performance seals and gaskets. The UV21 is a solvent free system and has an excellent six month shelf life at ambient temperatures.
Physical Properties Metric English Comments
Viscosity 32000 - 36000 cP

@Temperature 23.0 °C
32000 - 36000 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 20 - 25
20 - 25
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Transparent