Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3490 cP | 3490 cP | uncured |
Atom Adhesives AA-BOND 2170 Epoxy Adhesive AA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrate. A.. |