Material Notes:
AA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrate. AA-BOND 2170 is low viscosity and easy to apply, can cure at room temperature. AA-BOND 2170 is high technology epoxy was formulated for applications in the automotive, medial, aerospace, photonic and assembly industries and can be used anywhere that require excellent chemical fastening to plastic parts.Appearance: AmberCure Type: Heat cure or Room TemperatureBenefits:Low viscosityEasy to apply Mix Ratio by weight: 100:100/Resin:Hardener Substrates: All types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrateTypical Application: Automotive, Medical, Aerospace, Photonic, Assembly, industries, Also can be used anywhere that requires excellent chemical fastening to plastic parts.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Viscosity 3490 cP
3490 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Shear Strength 16.5 MPa
2400 psi
Lap, Alum to Alum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 10.0 °C
50.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60.0 min
60.0 min
uncured