Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 340000 cP | 340000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 340000 cP @Shear Rate 206 1/s, Temperature 200 °C |
340000 cP @Shear Rate 206 1/s, Temperature 392 °F |
ASTM D3835 |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |