Material Notes:
KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesSelective self adhesionNon adhesion to metalsInsert-molding and co-injection molding availableInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Viscosity 340000 cP
340000 cP
A
800000 cP
800000 cP
B
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength 8.30 MPa
1200 psi
Elongation at Yield 420 %
420 %
Tear Strength 38.0 kN/m
217 pli
Compression Set 9.0 %

@Temperature 200 °C,
Time 14400 sec
9.0 %

@Temperature 392 °F,
Time 4.00 hour
50 %

@Temperature 150 °C,
Time 3600 sec
50 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 102
T90 (248°F, ODR)
66
T10 (248°F, ODR)
Regulatory Testing Class VI