Viscosity 3.50e+7 cP
3.50e+7 cP
target viscosity before cure
3M Filtek™ Z250 Universal Restorative Dental Composite
3M™ Filtek™ Z250 universal restorative is an esthetic, light cured, radiopaque composite specifically designed for use in anterior or posterior direct or indirect restorations. Bonding to tooth s..