Material Notes:
3M™ Filtek™ Z250 universal restorative is an esthetic, light cured, radiopaque composite specifically designed for use in anterior or posterior direct or indirect restorations. Bonding to tooth structure is accomplished by using a dental adhesive system, such as 3M™ Single Bond or 3M™ Scotchbond Multi-Purpose Adhesive Systems. The restorative is available in a variety of shades and is packaged in traditional syringes and single dose capsules.The matrix of this composite is a resin consisting of BIS-GMA (Bisphenol A diglycidyl ether dimethacrylate), UDMA (urethane dimethacrylate), and Bis-EMA (Bisphenol A polyethylene glycol diether dimethacrylate). This light-cured resin is filled with 60% (volume) silica/zirconia. The filler particle size distribution is 0.01 µm to 3.5 µm with an average particle size of 0.6 µm.Filtek™ Z250 exhibits about 18% less volumetric shrinkage upon curing than 3M™ Z100™. An example from the manufacturer shows shrinkage of 2.0% after 5 minutes and 2.2% after 30 minutes; sample geometry will effect actual values. Wet fracture toughness is 1.5 MN/m. The wear rate in an in-vitro 3-body wear test gives 3.6 µLoss/39,000 cycles.Information provided by 3M. Contact 3M for further information before specifying or using this product.
Physical Properties Metric English Comments
Viscosity 3.50e+7 cP
3.50e+7 cP
target viscosity before cure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
Diametral tensile strength
Flexural Yield Strength 155 MPa
22500 psi
Flexural Modulus 11.0 GPa
1600 ksi
Compressive Yield Strength 405 MPa
58700 psi
Adhesive Bond Strength 24.0 MPa
3480 psi
for 2.5 mm increment. Bond strength to dentin using 3M Single Bond adhesive; C2 color
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
Light cured