Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.90e+6 - 3.30e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
2.90e+6 - 3.30e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF) Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically .. |
|||
Viscosity | 2.90e+6 - 3.30e+6 cP | 2.90e+6 - 3.30e+6 cP | Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF) Hylar® 301F is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.Features: High Viscosity; HomopolymerUses: Coating ApplicationsAdditiona.. |
|||
Viscosity | 2.90e+6 - 3.30e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
2.90e+6 - 3.30e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF) Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The disper.. |