Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Hylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and tough films that have a broad useful temperature range. These films are highly resistant to most environmental conditions including gamma radiation and are essentially transparent to ultraviolet radiation. The weathering characteristics of Hylar® 5000 coatings lead to excellent performance for the long term.Features: Clean/High Purity; Crystalline; Good Strength; Good Toughness; Good UV Resistance; Good Weather Resistance; High Molecular Weight; Low to No Odor; Radiation (Gamma) ResistantUses: Coating Applications; FilmAdditional Properties: 1% wt Loss (TGA) - TGA 382 to 393 °C; Hegman Grind - ASTM D1210 5.50 to 6.00; Moisture Content - < 0.50 %; Purity - > 99.5 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.75 - 1.77 g/cc
0.0632 - 0.0639 lb/in³
ASTM D792
Water Absorption at Saturation 0.040 %
0.040 %
ASTM D570
Viscosity 2.90e+6 - 3.30e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.90e+6 - 3.30e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Thermal Properties Metric English Comments
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Optical Properties Metric English Comments
Gloss >= 25 %
>= 25 %
60°; ASTM D2457
Descriptive Properties Value Comments
Availability Europe; North America
Color White
Form Powder
Processing Technique Coating