Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.15 cP | 3.15 cP | 96% Sulfuric Acid; ISO Test |
BASF Capron® B85ZP Nylon 6 (DAM) (America)
(discontinued **) Not Impact modified.Information provided by BASF.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Viscosity | 3.15 - 85.0 cP | 3.15 - 85.0 cP | Average value: 10.3 cP Grade Count:5 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |