Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 290000 cP | 290000 cP | Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Viscosity | 290000 cP | 290000 cP | Melt Viscosity, 200°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |