Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Viscosity | 245000 cP | 245000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |