Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2260 cP | 2260 cP | |
Abatron AboCast/AboCure 8110-2 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |