Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 220000 cP | 220000 cP | (#7spindle/10 rpm) |
Aptek 6505PMF Electronic-grade, non-conductive adhesive APTEK 6506-PMF is a one component, 100% solid, mineral-filled epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards as well as a protective barri.. |