Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 21000 cP | 21000 cP | Mixed (SSA #14/6R, 10 rpm) |
Tra-Con Tra-Coat WCC2B UV Curable Optical Adhesive TRA-COAT WCC2B is a clear, medium viscosity compound developed for optical fiber, glass, and general purpose bonding. This one-part liquid cures with exposure to UV light at 100 fpm under a 300 watt.. |