Viscosity 21000 cP
21000 cP
Mixed (SSA #14/6R, 10 rpm)
Tra-Con Tra-Coat WCC2B UV Curable Optical Adhesive
TRA-COAT WCC2B is a clear, medium viscosity compound developed for optical fiber, glass, and general purpose bonding. This one-part liquid cures with exposure to UV light at 100 fpm under a 300 watt..