Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.0 - 2.0 cP @Temperature 38.0 °C |
1.0 - 2.0 cP @Temperature 100 °F |
ASTM D445, DIN 51 561 |
Chesterton 775 Moisture Shield Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri.. |