Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.0 cP | 1.0 cP | |
ND Industries 624 Isopropyl Alcohol SuperGlue accelerator Very fast acting SuperGlue accelerator for plastic - 15 sec - Non-ozone depleting but flammable solvent |
|||
Viscosity | 1.0 cP | 1.0 cP | |
Permabond CSA-NF Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA-NF) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It significantly reduces t.. |
|||
Viscosity | <= 1.0 cP | <= 1.0 cP | |
Huntsman Araldite RD-1 Reactive Diluent Weight per Epoxide (EEW, g/eq) 140 to 160. Max color is 2.Comments/Applications: Butyl glycidyl ether - monofunctional epoxy. For use with liquid epoxy resins to lower their viscosity and improve .. |
|||
Viscosity | 1.0 - 5.0 cP | 1.0 - 5.0 cP | |
Huntsman DY 062 Epoxy Accelerator Mix Ratio with GY 6010 is 5.Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Benzyl dimethyl amine (BDMA)-tertiary amine accelerator. Com.. |
|||
Viscosity | <= 1.0 cP @Temperature 25.0 °C |
<= 1.0 cP @Temperature 77.0 °F |
|
LyondellBasell TBAcâ„¢ Solvent, Tertiary butyl acetate Information provided by Lyondell. |
|||
Viscosity | 1.0 cP @Temperature 20.0 °C |
1.0 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik 8036 Carboxymethylcellulose (CMC) Technical GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conc.. |
|||
Viscosity | 1.0 cP @Temperature 20.0 °C |
1.0 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik DTK/DTE Carboxymethylcellulose (CMC) Technical GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conc.. |
|||
Viscosity | 1.0 cP | 1.0 cP | |
Dow Corning HV 1860/120 PRIMER Primer designed for use with peroxide curing silicone rubbers to provide good bonding to metal, glass fibre and epoxy resinInformation provided by Dow Corning |
|||
Viscosity | 1.0 - 2.0 cP @Temperature 38.0 °C |
1.0 - 2.0 cP @Temperature 100 °F |
ASTM D445, DIN 51 561 |
Chesterton 775 Moisture Shield Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri.. |
|||
Viscosity | <= 1.0 cP | <= 1.0 cP | |
3M Scotch-Weld™ AC452 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC452 is acetone based and will attack some plastics.Information provided by 3M |
|||
Viscosity | 1.0 cP | 1.0 cP | 50-12 water-like viscosity |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |
|||
Viscosity | 1.0 cP | 1.0 cP | |
3M Scotch-Weld™ AC12 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC12 is isopropyl alcohol basedInformation provided by 3M |