Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1830 cP @Temperature 177 °C |
1830 cP @Temperature 350 °F |
Typical |
Bostik 2105 Low viscosity, short open time EVA Glue Stick Bostik 2105 Low viscosity, short open time EVA Glue StickLow viscosity. Short open time for woodworking and packaging applications. |