Bostik 2105 Low viscosity, short open time EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 2105 Low viscosity, short open time EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 2105 Low viscosity, short open time EVA Glue StickLow viscosity. Short open time for woodworking and packaging applications.
Physical Properties Metric English Comments
Viscosity 1830 cP

@Temperature 177 °C
1830 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 65.6 °C
150 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Processing Properties Metric English Comments
Pot Life 0.083 - 0.17 min
0.083 - 0.17 min
Open Time
Descriptive Properties Value Comments
Color Straw