Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 165000 cP | 165000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Viscosity | 165000 cP | 165000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Viscosity | 165000 cP | 165000 cP | Mixed; TM R050-12 |
Resinlab® EP1056LC Urethane Modified Epoxy Adhesive Resinlab™ EP1056LC is a two part urethane modified epoxy adhesive designed to give good adhesion to metals and hard to bond surfaces such as PVC. It is thixotropic to provide good gap filling abili.. |