Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1450 cP | 1450 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Viscosity | 1450 cP @Temperature -25.0 °C |
1450 cP @Temperature -13.0 °F |
Cold Crank |
ChevronTexaco 100R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Viscosity | 1450 cP @Temperature 180 °C |
1450 cP @Temperature 356 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail.. |
|||
Viscosity | 1450 cP @Temperature 40.0 °C |
1450 cP @Temperature 104 °F |
25% in dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Viscosity | 1450 cP | 1450 cP | |
Von Roll Isola IMI Varnish 74030 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >99°C. Usa.. |