Polymer Property : Viscosity = 145 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.73 - 145 cP
2.73 - 145 cP
Average value: 51.2 cP Grade Count:8
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..