Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 110 - 125 cP | 110 - 125 cP | ASTM D445 |
ExxonMobil Jayflex™ DIDP Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 68515-49-1EC Number: 271-091-4Information provided by ExxonMobil |
|||
Viscosity | 60 - 125 cP @Temperature 25.0 °C |
60 - 125 cP @Temperature 77.0 °F |
|
Abatron AboThane 8003-3 Polyurethane Coating AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, .. |
|||
Viscosity | 60 - 125 cP @Temperature 25.0 °C |
60 - 125 cP @Temperature 77.0 °F |
Uncured |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |