Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 12.0 - 950000 cP | 12.0 - 950000 cP | Average value: 118000 cP Grade Count:64 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |